Matching Items (17)
Filtering by

Clear all filters

155430-Thumbnail Image.png
Description
A new class of layered materials called the transition metal trichalcogenides (TMTCs) exhibit strong anisotropic properties due to their quasi-1D nature. These 2D materials are composed of chain-like structures which are weakly bound to form planar sheets with highly directional properties. The vibrational properties of three materials from the TMTC

A new class of layered materials called the transition metal trichalcogenides (TMTCs) exhibit strong anisotropic properties due to their quasi-1D nature. These 2D materials are composed of chain-like structures which are weakly bound to form planar sheets with highly directional properties. The vibrational properties of three materials from the TMTC family, specifically TiS3, ZrS3, and HfS3, are relatively unknown and studies performed in this work elucidates the origin of their Raman characteristics. The crystals were synthesized through chemical vapor transport prior to mechanical exfoliation onto Si/SiO¬2 substrates. XRD, AFM, and Raman spectroscopy were used to determine the crystallinity, thickness, and chemical signature of the exfoliated crystals. Vibrational modes and anisotropic polarization are investigated through density functional theory calculations and angle-resolved Raman spectroscopy. Particular Raman modes are explored in order to correlate select peaks to the b-axis crystalline direction. Mode III vibrations for TiS3, ZrS3, and HfS3 are shared between each material and serves as a unique identifier of the crystalline orientation in MX3 materials. Similar angle-resolved Raman studies were conducted on the novel Nb0.5Ti0.5S3 alloy material grown through chemical vapor transport. Results show that the anisotropy direction is more difficult to determine due to the randomization of quasi-1D chains caused by defects that are common in 2D alloys. This work provides a fundamental understanding of the vibrational properties of various TMTC materials which is needed to realize applications in direction dependent polarization and linear dichroism.
ContributorsKong, Wilson (Author) / Tongay, Sefaattin (Thesis advisor) / Wang, Liping (Committee member) / Green, Matthew (Committee member) / Arizona State University (Publisher)
Created2017
155871-Thumbnail Image.png
Description
Performance of photovoltaic (PV) modules decrease as the operating temperatures increase. In hot climatic conditions, the operating temperature can reach as high as 85°C for the rooftop modules. Considering a typical power drop of 0.5%/°C for crystalline silicon modules, a performance decrease of approximately 30% could be expected during peak

Performance of photovoltaic (PV) modules decrease as the operating temperatures increase. In hot climatic conditions, the operating temperature can reach as high as 85°C for the rooftop modules. Considering a typical power drop of 0.5%/°C for crystalline silicon modules, a performance decrease of approximately 30% could be expected during peak summer seasons due to the difference between module rated temperature of 25°C and operating temperature of 85°C. Therefore, it is critical to accurately predict the temperature of the modules so the performance can be accurately predicted. The module operating temperature is based not only on the ambient and irradiance conditions but is also based on the thermal properties of module packaging materials. One of the key packaging materials that would influence the module operating temperature is the substrate, polymer backsheet or glass. In this study, the thermal influence of three different polymer backsheet substrates and one glass substrate has been investigated through five tasks:

1. Determination and modeling of substrate or module temperature of coupons using four different substrates (three backsheet materials and one glass material).

2. Determination and modeling of cell temperature of coupons using four different substrates (three backsheet materials and one glass material)

3. Determination of temperature difference between cell and individual substrates for coupons of all four substrates

4. Determination of NOCT (nominal operating cell temperature) of coupons using all four substrate materials

5. Comparison of operating temperature difference between backsheet substrate coupons.

All these five tasks have been executed using the specially constructed one-cell coupons with identical cells but with four different substrates. For redundancy, two coupons per substrate were constructed and investigated. This study has attempted to model the effect of thermal conductivity of backsheet material on the cell and backsheet temperatures.
ContributorsNatarajan Rammohan, Balamurali (Author) / Tamizhmani, Govindasamy (Thesis advisor) / Srinivasan, Devarajan (Committee member) / Kuitche, Joseph (Committee member) / Arizona State University (Publisher)
Created2017
158450-Thumbnail Image.png
Description
In the current photovoltaic (PV) industry, the O&M (operations and maintenance) personnel in the field primarily utilize three approaches to identify the underperforming or defective modules in a string: i) EL (electroluminescence) imaging of all the modules in the string; ii) IR (infrared) thermal imaging of all the modules in

In the current photovoltaic (PV) industry, the O&M (operations and maintenance) personnel in the field primarily utilize three approaches to identify the underperforming or defective modules in a string: i) EL (electroluminescence) imaging of all the modules in the string; ii) IR (infrared) thermal imaging of all the modules in the string; and, iii) current-voltage (I-V) curve tracing of all the modules in the string. In the first and second approaches, the EL images are used to detect the modules with broken cells, and the IR images are used to detect the modules with hotspot cells, respectively. These two methods may identify the modules with defective cells only semi-qualitatively, but not accurately and quantitatively. The third method, I-V curve tracing, is a quantitative method to identify the underperforming modules in a string, but it is an extremely time consuming, labor-intensive, and highly ambient conditions dependent method. Since the I-V curves of individual modules in a string are obtained by disconnecting them individually at different irradiance levels, module operating temperatures, angle of incidences (AOI) and air-masses/spectra, all these measured curves are required to be translated to a single reporting condition (SRC) of a single irradiance, single temperature, single AOI and single spectrum. These translations are not only time consuming but are also prone to inaccuracy due to inherent issues in the translation models. Therefore, the current challenges in using the traditional I-V tracers are related to: i) obtaining I-V curves simultaneously of all the modules and substrings in a string at a single irradiance, operating temperature, irradiance spectrum and angle of incidence due to changing weather parameters and sun positions during the measurements, ii) safety of field personnel when disconnecting and reconnecting of cables in high voltage systems (especially field aged connectors), and iii) enormous time and hardship for the test personnel in harsh outdoor climatic conditions. In this thesis work, a non-contact I-V (NCIV) curve tracing tool has been integrated and implemented to address the above mentioned three challenges of the traditional I-V tracers.

This work compares I-V curves obtained using a traditional I-V curve tracer with the I-V curves obtained using a NCIV curve tracer for the string, substring and individual modules of crystalline silicon (c-Si) and cadmium telluride (CdTe) technologies. The NCIV curve tracer equipment used in this study was integrated using three commercially available components: non-contact voltmeters (NCV) with voltage probes to measure the voltages of substrings/modules in a string, a hall sensor to measure the string current and a DAS (data acquisition system) for simultaneous collection of the voltage data obtained from the NCVs and the current data obtained from the hall sensor. This study demonstrates the concept and accuracy of the NCIV curve tracer by comparing the I-V curves obtained using a traditional capacitor-based tracer and the NCIV curve tracer in a three-module string of c-Si modules and of CdTe modules under natural sunlight with uniform light conditions on all the modules in the string and with partially shading one or more of the modules in the string to simulate and quantitatively detect the underperforming module(s) in a string.
ContributorsMurali, Sanjay (Author) / Tamizhmani, Govindasamy (Thesis advisor) / Srinivasan, Devarajan (Committee member) / Rogers, Bradley (Committee member) / Arizona State University (Publisher)
Created2020
157910-Thumbnail Image.png
Description
The goal of any solar photovoltaic (PV) system is to generate maximum energy throughout its lifetime. The parameters that can affect PV module power output include: solar irradiance, temperature, soil accumulation, shading, encapsulant browning, encapsulant delamination, series resistance increase due to solder bond degradation and corrosion and shunt resistance decrease

The goal of any solar photovoltaic (PV) system is to generate maximum energy throughout its lifetime. The parameters that can affect PV module power output include: solar irradiance, temperature, soil accumulation, shading, encapsulant browning, encapsulant delamination, series resistance increase due to solder bond degradation and corrosion and shunt resistance decrease due to potential induced degradation, etc. Several PV modules together in series makes up a string, and in a power plant there are a number of these strings in parallel which can be referred to as an array. Ideally, PV modules in a string should be identically matched to attain maximum power output from the entire string. Any underperforming module or mismatch among modules within a string can reduce the power output. The goal of this project is to quickly identify and quantitatively determine the underperforming module(s) in an operating string without the use of an I-V curve tracer, irradiance sensor or temperature sensor. This goal was achieved by utilizing Radiovoltmeters (RVM). In this project, it is demonstrated that the voltages at maximum power point (Vmax) of all the individual modules in a string can be simultaneously and quantitatively obtained using RVMs at a single irradiance, single module operating temperature, single spectrum and single angle of incidence. By combining these individual module voltages (Vmax) with the string current (Imax) using a Hall sensor, the power output of individual modules can be obtained, quickly and quantitatively.
ContributorsTahghighi, Arash (Author) / Tamizhmani, Govindasamy (Thesis advisor) / Rogers, Bradley (Committee member) / Srinivasan, Devarajan (Committee member) / Arizona State University (Publisher)
Created2019
158822-Thumbnail Image.png
Description
Deformable heat exchangers could provide a multitude of previously untapped advantages ranging from adaptable performance via macroscale, dynamic shape change (akin to dilation/constriction seen in blood vessels) to enhanced heat transfer at thermal interfaces through microscale, surface deformations. So far, making deformable, ‘soft heat exchangers’ (SHXs) has been limited by

Deformable heat exchangers could provide a multitude of previously untapped advantages ranging from adaptable performance via macroscale, dynamic shape change (akin to dilation/constriction seen in blood vessels) to enhanced heat transfer at thermal interfaces through microscale, surface deformations. So far, making deformable, ‘soft heat exchangers’ (SHXs) has been limited by the low thermal conductivity of materials with suitable mechanical properties. The recent introduction of liquid-metal embedded elastomers by Bartlett et al1 has addressed this need. Specifically, by remaining soft and stretchable despite the addition of filler, these thermally conductive composites provide an ideal material for the new class of “soft thermal systems”, which is introduced in this work. Understanding such thermal systems will be a key element in enabling technology that require high levels of stretchability, such as thermoregulatory garments, soft electronics, wearable electronics, and high-powered robotics. Shape change inherent to SHX operation has the potential to violate many conventional assumptions used in HX design and thus requires the development of new theoretical approaches to predict performance. To create a basis for understanding these devices, this work highlights two sequential studies. First, the effects of transitioning to a surface deformable, SHX under steady state static conditions in the setting of a liquid cooling device for thermoregulation, electronics and robotics applications was explored. In this study, a thermomechanical model was built and validated to predict the thermal performance and a system wide analysis to optimize such devices was carried out. Second, from a more fundamental perspective, the effects of SHXs undergoing transient shape deformation during operation was explored. A phase shift phenomenon in cooling performance dependent on stretch rate, stretch extent and thermal diffusivity was discovered and explained. With the use of a time scale analysis, the extent of quasi-static assumption viability in modeling such systems was quantified and multiple shape modulation regime limits were defined. Finally, nuance considerations and future work of using liquid metal-silicone composites in SHXs were discussed.
ContributorsKotagama, Praveen (Author) / Rykaczewski, Konrad (Thesis advisor) / Wang, Robert (Committee member) / Phelan, Patrick (Committee member) / Herrmann, Marcus (Committee member) / Green, Matthew (Committee member) / Arizona State University (Publisher)
Created2020
156151-Thumbnail Image.png
Description
Alloying in semiconductors has enabled many civilian technologies in optoelectronic, photonic fields and more. While the phenomenon of alloying is well established in traditional bulk semiconductors, owing to vastly available ternary phase diagrams, the ability to alloy in 2D systems are less clear. Recently anisotropic materials such as ReS2 and

Alloying in semiconductors has enabled many civilian technologies in optoelectronic, photonic fields and more. While the phenomenon of alloying is well established in traditional bulk semiconductors, owing to vastly available ternary phase diagrams, the ability to alloy in 2D systems are less clear. Recently anisotropic materials such as ReS2 and TiS3 have been extensively studied due to their direct-gap semiconductor and high mobility behaviors. This work is a report on alloys of ReS2 & ReSe2 and TiS3 &TiSe3.

Alloying selenium into ReS2 in the creation of ReS2xSe2-x, tunes the band gap and changes its vibrational spectrum. Depositing this alloy using bottom up approach has resulted in the loss of crystallinity. This loss of crystallinity was evidenced by grain boundaries and point defect shown by TEM images.

Also, in the creation of TiS3xSe3-x, by alloying Se into TiS3, a fixed ratio of 8% selenium deposit into TiS3 host matrix is observed. This is despite the vastly differing precursor amounts and growth temperatures, as evinced by detailed TEM, EDAX, TEM diffraction, and Raman spectroscopy measurements. This unusual behavior contrasts with other well-known layered material systems such as MoSSe, WMoS2 where continuous alloying can be attained. Cluster expansion theory calculations suggest that only limited composition (x) can be achieved. Considering the fact that TiSe3 vdW crystals have not been synthesized in the past, these alloying rejections can be attributed to energetic instability in the ternary phase diagrams estimated by calculations performed. Overall findings highlight potential means and challenges in achieving stable alloying in promising direct gap and high carrier mobility TiS3 materials.
ContributorsAgarwal, Ashutosh (Author) / Tongay, Sefaattin (Thesis advisor) / Green, Matthew (Committee member) / Zhuang, Houlong (Committee member) / Arizona State University (Publisher)
Created2018
155732-Thumbnail Image.png
Description
This is a two-part thesis. Part 1 presents the seasonal and tilt angle dependence of soiling loss factor of photovoltaic (PV) modules over two years for Mesa, Arizona (a desert climatic condition). Part 2 presents the development of an indoor artificial soil deposition chamber replicating natural dew cycle.

This is a two-part thesis. Part 1 presents the seasonal and tilt angle dependence of soiling loss factor of photovoltaic (PV) modules over two years for Mesa, Arizona (a desert climatic condition). Part 2 presents the development of an indoor artificial soil deposition chamber replicating natural dew cycle. Several environmental factors affect the performance of PV systems including soiling. Soiling on PV modules results in a decrease of sunlight reaching the solar cell, thereby reducing the current and power output. Dust particles, air pollution particles, pollen, bird droppings and other industrial airborne particles are some natural sources that cause soiling. The dust particles vary from one location to the other in terms of particle size, color, and chemical composition. The thickness and properties of the soil layer determine the optical path of light through the soil/glass interface. Soil accumulation on the glass surface is also influenced by environmental factors such as dew, wind speeds and rainfall. Studies have shown that soil deposition is closely related to tilt angle and exposure period before a rain event. The first part of this thesis analyzes the reduction in irradiance transmitted to a solar cell through the air/soil/glass in comparison to a clean cell (air/glass interface). A time series representation is used to compare seasonal soiling loss factors for two consecutive years (2014-2016). The effect of tilt angle and rain events on these losses are extensively analyzed. Since soiling is a significant field issue, there is a growing need to address the problem, and several companies have come up with solutions such as anti-soiling coatings, automated cleaning systems etc. To test and validate the effectiveness of these anti-soiling coating technologies, various research institutes around the world are working on the design and development of artificial indoor soiling chambers to replicate the natural process in the field. The second part of this thesis work deals with the design and development of an indoor artificial soiling chamber that replicates natural soil deposition process in the field.
ContributorsVirkar, Shalaim (Author) / Tamizhmani, Govindasamy (Thesis advisor) / Srinivasan, Devarajan (Committee member) / Kuitche, Joseph (Committee member) / Arizona State University (Publisher)
Created2017