In recent years, an increase of environmental temperature in urban areas has raised many concerns. These areas are subjected to higher temperature compared to the rural surrounding areas. Modification of land surface and the use of materials such as concrete and/or asphalt are the main factors influencing the surface energy balance and therefore the environmental temperature in the urban areas. Engineered materials have relatively higher solar energy absorption and tend to trap a relatively higher incoming solar radiation. They also possess a higher heat storage capacity that allows them to retain heat during the day and then slowly release it back into the atmosphere as the sun goes down. This phenomenon is known as the Urban Heat Island (UHI) effect and causes an increase in the urban air temperature. Many researchers believe that albedo is the key pavement affecting the urban heat island. However, this research has shown that the problem is more complex and that solar reflectivity may not be the only important factor to evaluate the ability of a pavement to mitigate UHI. The main objective of this study was to analyze and research the influence of pavement materials on the near surface air temperature. In order to accomplish this effort, test sections consisting of Hot Mix Asphalt (HMA), Porous Hot Mix asphalt (PHMA), Portland Cement Concrete (PCC), Pervious Portland Cement Concrete (PPCC), artificial turf, and landscape gravels were constructed in the Phoenix, Arizona area. Air temperature, albedo, wind speed, solar radiation, and wind direction were recorded, analyzed and compared above each pavement material type. The results showed that there was no significant difference in the air temperature at 3-feet and above, regardless of the type of the pavement. Near surface pavement temperatures were also measured and modeled. The results indicated that for the UHI analysis, it is important to consider the interaction between pavement structure, material properties, and environmental factors. Overall, this study demonstrated the complexity of evaluating pavement structures for UHI mitigation; it provided great insight on the effects of material types and properties on surface temperatures and near surface air temperature.
Perpetual Pavements, if properly designed and rehabilitated, it can last longer than 50 years without major structural rehabilitation. Fatigue endurance limit is a key parameter for designing perpetual pavements to mitigate bottom-up fatigue cracking. The endurance limit has not been implemented in the Mechanistic Empirical Pavement Design Guide software, currently known as DARWin-ME. This study was conducted as part of the National Cooperative Highway Research Program (NCHRP) Project 9-44A to develop a framework and mathematical methodology to determine the fatigue endurance limit using the uniaxial fatigue test. In this procedure, the endurance limit is defined as the allowable tensile strains at which a balance takes place between the fatigue damage during loading, and the healing during the rest periods between loading pulses. The viscoelastic continuum damage model was used to isolate time dependent damage and healing in hot mix asphalt from that due to fatigue. This study also included the development of a uniaxial fatigue test method and the associated data acquisition computer programs to conduct the test with and without rest period. Five factors that affect the fatigue and healing behavior of asphalt mixtures were evaluated: asphalt content, air voids, temperature, rest period and tensile strain. Based on the test results, two Pseudo Stiffness Ratio (PSR) regression models were developed. In the first model, the PSR was a function of the five factors and the number of loading cycles. In the second model, air voids, asphalt content, and temperature were replaced by the initial stiffness of the mix. In both models, the endurance limit was defined when PSR is equal to 1.0 (net damage is equal to zero). The results of the first model were compared to the results of a stiffness ratio model developed based on a parallel study using beam fatigue test (part of the same NCHRP 9-44A). The endurance limit values determined from uniaxial and beam fatigue tests showed very good correlation. A methodology was described on how to incorporate the second PSR model into fatigue analysis and damage using the DARWin-ME software. This would provide an effective and efficient methodology to design perpetual flexible pavements.
Asphalt concrete is the most recycled material in the United States and its reclamation allows the positive reuse of the constituent aggregates and asphalt binder, contributing to the long-term sustainability of the transportation infrastructure; decreasing costs, and the total energy and greenhouse emissions embodied into new materials and infrastructure. Although the national trends in Reclaimed Asphalt Pavements (RAP) usage are encouraging, the environmental conditions in Phoenix, Arizona are extreme and needs further consideration.
The objective of this research study was to evaluate the viability of using RAP in future pavement maintenance and rehabilitation projects for the City. Agencies in the State of Arizona have been slow adopting the use of RAP as a regular practice. While the potential benefits are great, there is some concern on the impact to long-term pavement performance.
RAP millings were sampled from the city’s stockpiles; processed RAP and virgin materials were provided by a local plant. Two asphalt binders were used: PG 70-10 and PG 64-16. RAP variability was evaluated by aggregate gradations; extracted and recovered binder was tested for properties and grading.
A mixture design procedure based on the City’s specifications was defined to establish trial blends. RAP incorporation was based on national and local practices. Four different RAP contents were studied 10%, 15%, 25%, and 25% content with a softer binder, in addition to a control mix (0% RAP).
Performance tests included: dynamic modulus to evaluate stiffness; Flow Number, to assess susceptibility for permanent deformation (rutting); and Tensile Strength Ratio as a measure of susceptibility to moisture damage.
Binder testing showed very stiff recovered asphalts and variable contents with a reasonable variability on aggregate gradations. Performance test results showed slightly higher modulus as RAP content increases, showing a slight improvement related to rutting as well. For moisture damage potential, all mixtures performed well showing improvement for RAP mixtures in most cases.
Statistical analysis showed that 0%, 10%, 15% and 25% with softer binder do not present significant statistical difference among mixtures, indicating that moderate RAP contents are feasible to use within the City paving operations and will not affect greatly nor negatively the pavement performance.
Six asphalt mixes were prepared with three RAP contents, 0%, 15% and 25%, with and without Organosilane. The mixing temperature was reduced by 10°C and the compaction temperature was reduced by 30°C. Mix designs were performed, and the volumetric properties were compared. The mixture laboratory performance was evaluated for all mixtures by conducting Dynamic Modulus, Flow Number and Tensile Strength Ratio tests.
The study findings showed that mixtures achieved better compaction at a reduced temperature of 30°C. Mixtures modified with Organosilane generally exhibited softer behavior at the extreme ends of lower and higher temperatures. The lower moduli are to reduce the potential for cracking. For the Flow Number test, the RAP mixtures with OS passed the minimum required at all traffic levels. Tensile Strength Ratio results increased with the increase in RAP percentage, and further increase was observed when OS was used. The OS reduced the sticking nature of the binder to the molds and equipment, which reduced the efforts in cleaning them.
Finally, the future use of RAP by the City of Phoenix would positively contributes to their sustainability aspiration and initiatives. The use of Organosilane may even facilitates higher percentage of RAP usage; it definitely improves the moisture resistance of asphalt mixtures, especially when lower mixing and compaction temperatures are desired or used.