Matching Items (27)
157332-Thumbnail Image.png
Description
In the past, the photovoltaic (PV) modules were typically constructed with glass superstrate containing cerium oxide and EVA (ethylene vinyl acetate) encapsulant containing UV absorbing additives. However, in the current industry, the PV modules are generally constructed without cerium oxide in the glass and UV absorbing additives in EVA to

In the past, the photovoltaic (PV) modules were typically constructed with glass superstrate containing cerium oxide and EVA (ethylene vinyl acetate) encapsulant containing UV absorbing additives. However, in the current industry, the PV modules are generally constructed without cerium oxide in the glass and UV absorbing additives in EVA to increase quantum efficiency of crystalline silicon solar cells in the UV regions. This new approach is expected to boost the initial power output of the modules and reduce the long-term encapsulant browning issues. However, this new approach could lead to other durability and reliability issues such as delamination of encapsulant by damaging interfacial bonds, destruction of antireflection coating on solar cells and even breakage of polymeric backbone of EVA. This work compares the durability and reliability issues of PV modules having glass without cerium oxide and EVA with (aka, UVcut or UVC) and without (aka, UVpass or UVP) UV absorbing additives. In addition, modules with UVP front and UVC back EVA have also been investigated (aka, UVhybrid or UVH). The mini-modules with nine split cells used in this work were fabricated at ASU’s Photovoltaic Reliability Laboratory. The durability and reliability caused by three stress variables have been investigated and the three variables are temperature, humidity/oxygen and UV dosage. The influence of up to 800 kWh/m2 UV dosage has been investigated at various dosage levels. Many material and device characterizations have been performed to ascertain the degradation modes and effects. The UVC modules showed encapsulant discoloration at the cell centers as expected but the UVH modules showed a ring-shaped encapsulant discoloration close to the cell edges as evidenced in the UV fluorescence (UVF) imaging study. The PV modules containing UVP on both sides of cells with limited access to humidity or oxygen through backsheet (covered backsheet with adhesive aluminum tape) seem to experience encapsulant delamination as evidenced in the UVF images. Plausible explanations for these observations have been presented.
ContributorsArularasu, Pooja (Author) / Tamizhmani, Govindasamy (Thesis advisor) / Mu, Bin (Thesis advisor) / Varman, Arul M (Committee member) / Arizona State University (Publisher)
Created2019
157255-Thumbnail Image.png
Description
Rapid development of new technology has significantly disrupted the way radiotherapy is planned and delivered. These processes involve delivering high radiation doses to the target tumor while minimizing dose to the surrounding healthy tissue. However, with rapid implementation of these new technologies, there is a need for the detection of

Rapid development of new technology has significantly disrupted the way radiotherapy is planned and delivered. These processes involve delivering high radiation doses to the target tumor while minimizing dose to the surrounding healthy tissue. However, with rapid implementation of these new technologies, there is a need for the detection of prescribed ionizing radiation for radioprotection of the patient and quality assurance of the technique employed. Most available clinical sensors are subjected to various limitations including requirement of extensive training, loss of readout with sequential measurements, sensitivity to light and post-irradiation wait time prior to analysis. Considering these disadvantages, there is still a need for a sensor that can be fabricated with ease and still operate effectively in predicting the delivered radiation dose.



The dissertation discusses the development of a sensor that changes color upon exposure to therapeutic levels of ionizing radiation used during routine radiotherapy. The underlying principle behind the sensor is based on the formation of gold nanoparticles from its colorless precursor salt solution upon exposure to ionizing radiation. Exposure to ionizing radiation generates free radicals which reduce ionic gold to its zerovalent gold form which further nucleate and mature into nanoparticles. The generation of these nanoparticles render a change in color from colorless to a maroon/pink depending on the intensity of incident ionizing radiation. The shade and the intensity of the color developed is used to quantitatively and qualitatively predict the prescribed radiation dose.

The dissertation further describes the applicability of sensor to detect a wide range of ionizing radiation including high energy photons, protons, electrons and emissions from radioactive isotopes while remaining insensitive to non-ionizing radiation. The sensor was further augmented with a capability to differentiate regions that are irradiated and non-irradiated in two dimensions. The dissertation further describes the ability of the sensor to predict dose deposition in all three dimensions. The efficacy of the sensor to predict the prescribed dose delivered to canine patients undergoing radiotherapy was also demonstrated. All these taken together demonstrate the potential of this technology to be translatable to the clinic to ensure patient safety during routine radiotherapy.
ContributorsSubramaniam Pushpavanam, Karthik (Author) / Rege, Kaushal (Thesis advisor) / Sapareto, Stephen (Committee member) / Nannenga, Brent (Committee member) / Green, Matthew (Committee member) / Mu, Bin (Committee member) / Arizona State University (Publisher)
Created2019
157001-Thumbnail Image.png
Description
Ethylene vinyl acetate (EVA) is the most commonly used encapsulant in photovoltaic modules. However, EVA degrades over time and causes performance losses in PV system. Therefore, EVA degradation is a matter of concern from a durability point of view.

This work compares EVA encapsulant degradation in glass/backsheet and glass/glass field-aged

Ethylene vinyl acetate (EVA) is the most commonly used encapsulant in photovoltaic modules. However, EVA degrades over time and causes performance losses in PV system. Therefore, EVA degradation is a matter of concern from a durability point of view.

This work compares EVA encapsulant degradation in glass/backsheet and glass/glass field-aged PV modules. EVA was extracted from three field-aged modules (two glass/backsheet and one glass/glass modules) from three different manufacturers from various regions (cell edges, cell centers, and non-cell region) from each module based on their visual and UV Fluorescence images. Characterization techniques such as I-V measurements, Colorimetry, Different Scanning Calorimetry, Thermogravimetric Analysis, Raman spectroscopy, and Fourier Transform Infrared Spectroscopy were performed on EVA samples.

The intensity of EVA discoloration was quantified using colorimetric measurements. Module performance parameters like Isc and Pmax degradation rates were calculated from I-V measurements. Properties such as degree of crystallinity, vinyl acetate content and degree of crosslinking were calculated from DSC, TGA, and Raman measurements, respectively. Polyenes responsible for EVA browning were identified in FTIR spectra.

The results from the characterization techniques confirmed that when EVA undergoes degradation, crosslinking in EVA increases beyond 90% causing a decrease in the degree of crystallinity and an increase in vinyl acetate content of EVA. Presence of polyenes in FTIR spectra of degraded EVA confirmed the occurrence of Norrish II reaction. However, photobleaching occurred in glass/backsheet modules due to the breathable backsheet whereas no photobleaching occurred in glass/glass modules because they were hermetically sealed. Hence, the yellowness index along with the Isc and Pmax degradation rates of EVA in glass/glass module is higher than that in glass/backsheet modules.

The results implied that more acetic acid was produced in the non-cell region due to its double layer of EVA compared to the front EVA from cell region. But, since glass/glass module is hermetically sealed, acetic acid gets entrapped inside the module further accelerating EVA degradation whereas it diffuses out through backsheet in glass/backsheet modules. Hence, it can be said that EVA might be a good encapsulant for glass/backsheet modules, but the same cannot be said for glass/glass modules.
ContributorsPatel, Aesha Parimalbhai (Author) / Tamizhmani, Govindasamy (Thesis advisor) / Green, Matthew (Committee member) / Mu, Bin (Committee member) / Arizona State University (Publisher)
Created2018
157078-Thumbnail Image.png
Description
A new type of electronics was envisioned, namely edible electronics. Edible electronics are made by Food and Drug Administration (FDA) certified edible materials which can be eaten and digested by human body. Different from implantable electronics, test or treatment using edible electronics doesn’t require operations and perioperative complications.

This dissertation

A new type of electronics was envisioned, namely edible electronics. Edible electronics are made by Food and Drug Administration (FDA) certified edible materials which can be eaten and digested by human body. Different from implantable electronics, test or treatment using edible electronics doesn’t require operations and perioperative complications.

This dissertation bridges the food industry, material sciences, device fabrication, and biomedical engineering by demonstrating edible supercapacitors and electronic components and devices such as pH sensor.

Edible supercapacitors were fabricated using food materials from grocery store. 5 of them were connected in series to power a snake camera. Tests result showed that the current generated by supercapacitor have the ability to kill bacteria. Next more food, processed food and non-toxic level electronic materials were investigated. A “preferred food kit” was created for component fabrication based on the investigation. Some edible electronic components, such as wires, resistor, inductor, etc., were developed and characterized utilizing the preferred food kit. These components make it possible to fabricate edible electronic/device in the future work. Some edible electronic components were integrated into an edible electronic system/device. Then edible pH sensor was introduced and fabricated. This edible pH sensor can be swallowed and test pH of gastric fluid. PH can be read in a phone within seconds after the pH sensor was swallowed. As a side project, an edible double network gel electrolyte was synthesized for the edible supercapacitor.
ContributorsXu, Wenwen (Author) / Jiang, Hanqing (Thesis advisor) / Dai, Lenore (Committee member) / Green, Matthew (Committee member) / Mu, Bin (Committee member) / Yu, Hongbin (Committee member) / Arizona State University (Publisher)
Created2019
133572-Thumbnail Image.png
Description
Separation of carbon dioxide and methane for the upgrade of natural gas through use of pressure swing adsorption could potentially save large amounts of energy from the current, costly process of cryogenic distillation and provides greater cost effectiveness for carbon dioxide capture, and provide larger product flowrates than membrane permeation

Separation of carbon dioxide and methane for the upgrade of natural gas through use of pressure swing adsorption could potentially save large amounts of energy from the current, costly process of cryogenic distillation and provides greater cost effectiveness for carbon dioxide capture, and provide larger product flowrates than membrane permeation separation. The purpose of this study is to analyze the effects of varying initial conditions of a MatLab simulation, courtesy of Mai Xu, a graduate student at ASU, designed to use Langmuir isotherms, mass transfer equations, and adsorbent and gas properties to simulate a pressure swing adsorption process with a mixture of methane and carbon dioxide gas feed. The effects that will be varied are the adsorption/desorption time, pressurization/depressurization time, adsorption feed composition, desorption purge composition, adsorption pressure, desorption pressure, adsorption flow rate, and desorption flow rate. The study found that the trends in methane purity and production generally follow the trends predicted by literature and relevant equations, with pressure boundaries being the largest impacting factor. In addition there was a markedly inverse correlation between purity of methane product and the productivity of the system. This trend was only violated in one instance, at very low vacuum pressure during desorption, which could indicate an area that requires further study. Overall, the main areas of improvement in pressure swing adsorption for this system would be improving the selectivity of adsorption of carbon dioxide over methane, which requires improvement and change of the adsorbent, and more extreme vacuum pressures during desorption, both of which will increase methane yield and reduce operating costs.
ContributorsCook, Alexander Charles (Author) / Deng, Shuguang (Thesis director) / Mu, Bin (Committee member) / Chemical Engineering Program (Contributor) / Barrett, The Honors College (Contributor)
Created2018-05
134902-Thumbnail Image.png
Description
Metal-organic frameworks (MOFs) are a new set of porous materials comprised of metals or metal clusters bonded together in a coordination system by organic linkers. They are becoming popular for gas separations due to their abilities to be tailored toward specific applications. Zirconium MOFs in particular are known for their

Metal-organic frameworks (MOFs) are a new set of porous materials comprised of metals or metal clusters bonded together in a coordination system by organic linkers. They are becoming popular for gas separations due to their abilities to be tailored toward specific applications. Zirconium MOFs in particular are known for their high stability under standard temperature and pressure due to the strength of the Zirconium-Oxygen coordination bond. However, the acid modulator needed to ensure long range order of the product also prevents complete linker deprotonation. This leads to a powder product that cannot easily be incorporated into continuous MOF membranes. This study therefore implemented a new bi-phase synthesis technique with a deprotonating agent to achieve intergrowth in UiO-66 membranes. Crystal intergrowth will allow for effective gas separations and future permeation testing. During experimentation, successful intergrown UiO-66 membranes were synthesized and characterized. The degree of intergrowth and crystal orientations varied with changing deprotonating agent concentration, modulator concentration, and ligand:modulator ratios. Further studies will focus on achieving the same results on porous substrates.
ContributorsClose, Emily Charlotte (Author) / Mu, Bin (Thesis director) / Shan, Bohan (Committee member) / Chemical Engineering Program (Contributor) / Barrett, The Honors College (Contributor)
Created2016-12
134977-Thumbnail Image.png
Description
Polymer-nanoparticle composites (PNCs) show improved chemical and physical properties compared to pure polymers. However, nanoparticles dispersed in a polymer matrix tend to aggregate due to strong interparticle interactions. Electrospun nanofibers impregnated with nanoparticles have shown improved dispersion of nanoparticles. Currently, there are few models for quantifying dispersion in a PNC,

Polymer-nanoparticle composites (PNCs) show improved chemical and physical properties compared to pure polymers. However, nanoparticles dispersed in a polymer matrix tend to aggregate due to strong interparticle interactions. Electrospun nanofibers impregnated with nanoparticles have shown improved dispersion of nanoparticles. Currently, there are few models for quantifying dispersion in a PNC, and none for electrospun PNC fibers. A simulation model was developed to quantify the effects of nanoparticle volume loading and fiber to particle diameter ratios on the dispersion in a nanofiber. The dispersion was characterized using the interparticle distance along the fiber. Distributions of the interparticle distance were fit to Weibull distributions and a two-parameter empirical equation for the mean and standard deviation was found. A dispersion factor was defined to quantify the dispersion along the polymer fiber. This model serves as a standard for comparison for future experimental studies through its comparability with microscopy techniques, and as way to quantify and predict dispersion in polymer-nanoparticle electrospinning systems with a single performance metric.
ContributorsBalzer, Christopher James (Author) / Mu, Bin (Thesis director) / Armstrong, Mitchell (Committee member) / Chemical Engineering Program (Contributor) / Barrett, The Honors College (Contributor)
Created2016-12
154753-Thumbnail Image.png
Description
The problem of catastrophic damage purveys in any material application, and minimizing its occurrence is paramount for general health and safety. Thus, novel damage detection schemes are required that can sense the precursors to damage. Mechanochemistry is the area of research that involves the use of mechanical force to induce

The problem of catastrophic damage purveys in any material application, and minimizing its occurrence is paramount for general health and safety. Thus, novel damage detection schemes are required that can sense the precursors to damage. Mechanochemistry is the area of research that involves the use of mechanical force to induce a chemical change, with recent study focusing on directing the mechanical force to embedded mechanophore units for a targeted chemical response. Mechanophores are molecular units that provide a measureable signal in response to an applied force, often in the form of a visible color change or fluorescent emission, and their application to thermoset network polymers has been limited. Following preliminary work on polymer blends of cyclobutane-based mechanophores and epoxy, dimeric 9-anthracene carboxylic acid (Di-AC)-based mechanophore particles were synthesized and employed to form stress sensitive particle reinforced epoxy matrix composites.

Under an applied stress, the cyclooctane-rings in the Di-AC particles revert back to their fluorescent anthracene form, which linearly enhances the overall fluorescence of the composite in response to the applied strain. The fluorescent signal further allows for stress sensing in the elastic region of the stress-strain curve, which is considered to be a form of damage precursor detection. This behavior was further analyzed at the molecular scale with corresponding molecular dynamics simulations. Following the successful application of Di-AC to an epoxy matrix, the mechanophore particles were incorporated into a polyurethane matrix to show the universal nature of Di-AC as a stress-sensitive particle filler. Interestingly, in polyurethane Di-AC could successfully detect damage with less applied strain compared to the epoxy system.

While mechanophores of varying chemistries have been covalently incorporated into elastomeric and thermoplastic polymer systems, they have not yet been covalently incorporated a thermoset network polymer. Thus, following the study of mechanophore particles as stress-sensitive fillers, two routes of grafting mechanophore units into an epoxy system to form a self-sensing nanocomposite were explored. These involved the mechanophore precursor and mechanophore, cinnamamide and di-cinnamamide, respectively. With both molecules, the free amine groups can directly bond to epoxy resin to covalently incorporate themselves within the thermoset network to form a self-sensing nanocomposite.
ContributorsNofen, Elizabeth (Author) / Dai, Lenore L (Thesis advisor) / Chattopadhyay, Aditi (Thesis advisor) / Emady, Heather (Committee member) / Mu, Bin (Committee member) / Nielsen, David (Committee member) / Arizona State University (Publisher)
Created2016
154799-Thumbnail Image.png
Description
While the solution diffusion model and pore flow model dominate pervaporation transport mechanism modeling, a new model combining the solution diffusion and viscous flow models is validated using membranes with large scale defects exceeding 2 nm in diameter. A range of membranes was characterized using scanning electron microscopy and

While the solution diffusion model and pore flow model dominate pervaporation transport mechanism modeling, a new model combining the solution diffusion and viscous flow models is validated using membranes with large scale defects exceeding 2 nm in diameter. A range of membranes was characterized using scanning electron microscopy and x-ray diffraction (XRD) to determine quality and phase characteristics. MFI zeolite membranes of He/SF6 pure gas permeation ideal selectivities of 25, 15, and 3 for good, medium, and poor quality membranes were subjected to liquid pervaporations with a 5% ethanol in water feed, by weight. Feed pressure was increased from 1 to 5 atm, to validate existence of viscous flow in the defects. Component molar flux is modeled using the solution diffusion model and the viscous flow model, via J_i=F_i (γ_i x_i P_i^sat )+(ρ )/M_W ∅/μ_ij x_i P_h. A negative coefficient of thermal expansion is observed as permeances drop as a function of temperature in all three membranes, where ϕ=((ϵr_p^2)/τ∆x). Experimental parameter ϕ increased as a function of temperature, and increased with decreasing membrane quality. This further proves that zeolitic pores are shrinking in one direction, and pulling intercrystalline voids larger, increasing the (ϵ/τ) ratio. Permiabilities of the bad, medium, and good quality membrane also decreased over time for both ethanol and water, meaning that fundamental membrane characteristics changed as a function of temperature. To conclude, the model reasonably fits empirical data reasonably well.
ContributorsWilliams, Suzanne Jean (Author) / Lin, Jerry Y.S. (Thesis advisor) / Emady, Heather (Committee member) / Mu, Bin (Committee member) / Arizona State University (Publisher)
Created2016
155117-Thumbnail Image.png
Description
Ionic liquids (ILs), or low-temperature liquid salts, are a class of materials with unique and useful properties. Made up entirely of ions, ILs are remarkably tunable and diverse as cations and anions can be mixed and matched to yield desired properties. Because of this, IL/water systems range widely—from homogeneous mixtures

Ionic liquids (ILs), or low-temperature liquid salts, are a class of materials with unique and useful properties. Made up entirely of ions, ILs are remarkably tunable and diverse as cations and anions can be mixed and matched to yield desired properties. Because of this, IL/water systems range widely—from homogeneous mixtures to multiphasic systems featuring ionic liquid/liquid interfaces. Even more diversity is added when particles are introduced to these systems, as hard particles or soft-matter microgels interact with both ILs and water in complex ways. This work examines both miscible ionic liquid/water mixture and two-phase, immiscible ionic liquid/water systems. Extensive molecular dynamics (MD) simulations are utilized in conjunction with physical measurements to inform theoretical understanding of the nature of these systems, and this theoretical understanding is related to practical applications—in particular, the development of a low-temperature liquid electrolyte for use in molecular electronic transducer (MET) seismometers, and particle self-assembly and transport at ionic liquid/liquid interfaces such as those in Pickering emulsions.

The homogenous mixture of 1-butyl-3-methylimidazolium iodide and water is examined extensively through MD as well as physical characterization of properties. Molecular ordering within the liquid mixture is related to macroscopic properties. These mixtures are then used as the basis of an electrolyte with unusual characteristics, specifically a wide liquid temperature range with an extremely low lower bound combined with relatively low viscosity allowing excellent performance in the MET sensor. Electrolyte performance is further improved by the addition of fullerene nanoparticles, which dramatically increase device sensitivity. The reasons behind this effect are explored by testing the effect of graphene surface size and through MD simulations of fullerene and a silica nanoparticle (for contrast) in [BMIM][I]/water mixtures.

Immiscible ionic liquid/water systems are explored through MD studies of particles at IL/water interfaces. By increasing the concentration of hydrophobic nanoparticles at the IL/water interface, one study discovers the formation of a commingled IL/water/particle pseudo-phase, and relates this discovery to previously-observed unique behaviors of these interfaces, particularly spontaneous particle transport across the interface. The other study demonstrates that IL hydrophobicity can influence the deformation of thermo-responsive soft particles at the liquid/liquid interface.
ContributorsNickerson, Stella Day (Author) / Dai, Lenore L (Thesis advisor) / Yu, Hongyu (Committee member) / Lind, Mary Laura (Committee member) / Mu, Bin (Committee member) / Emady, Heather (Committee member) / Arizona State University (Publisher)
Created2016