Matching Items (4)
Filtering by

Clear all filters

137466-Thumbnail Image.png
Description
Dry and steam NanoBonding™ are conceived and researched to bond Si-based surfaces, via nucleation and growth of a two-dimensional SiOxHy or hydrated SiOxHy interphase connecting surfaces at the nanoscale across macroscopic domains. The motivation is to create strong, long lasting, hermetically bonded sensors with their electronics for the development

Dry and steam NanoBonding™ are conceived and researched to bond Si-based surfaces, via nucleation and growth of a two-dimensional SiOxHy or hydrated SiOxHy interphase connecting surfaces at the nanoscale across macroscopic domains. The motivation is to create strong, long lasting, hermetically bonded sensors with their electronics for the development of an artificial pancreas and to bond solar cells to glass panels for robust photovoltaic technology. The first step in NanoBonding™ is to synthesize smooth surfaces with 20 nm wide atomic terraces via a precursor phase, ß-cSiO2 on Si(100) and oxygen-deficient SiOx on the silica using the Herbots-Atluri process and Entrepix’s spin etching. Smooth precursor phases act as geometric and chemical template to nucleate and grow macroscopic contacting domains where cross bridging occurs via arrays of molecular strands in the hydrated SiOxHy interphase. Steam pressurization is found to catalyze NanoBonding™ consistently, eliminating the need for direct mechanical compression that limits the size and shape of wafers to be bonded in turn, reducing the cost of processing. Total surface energy measurements via 3 Liquids Contact Angle Analysis (3L CAA) enables accurate quantitative analysis of the total surface energy and each of its components. 3L CAA at each step in the process shows that surface energy drops to 42.4 ± 0.6 mJ/m2 from 57.5 ± 1.4 mJ/m2 after the Herbots-Atluri clean of an “As Received” wafer. 3L CAA after steam pressurization Nanobonding™ shows almost complete elimination from 13.8 mJ/m2 ± 1.0 to 0.002 ±- 0.0002 mJ/m2 in the contribution of acceptors to the total free surface energy, and an increase from 0.2 ± .03 to 23.8± 1.6 mJ/m2 in the contribution of donors. This is consistent with an increase in hydroxylation of the ß-cSiO2 surface as a consistent precursor phase for cross-bridging. This research optimizes the use of glycerin, water, and α-bromo-naphtalene in the use of 3L CAA to effectively quantify the components of total free surface energy which helps to better understand the most consistent method for NanoBonding™.
ContributorsBennett-Kennett, Ross Buchanan (Author) / Culbertson, Robert (Thesis director) / Herbots, Nicole (Committee member) / Foy, Joseph (Committee member) / Barrett, The Honors College (Contributor) / Materials Science and Engineering Program (Contributor) / Department of Physics (Contributor) / School of Historical, Philosophical and Religious Studies (Contributor)
Created2013-05
148168-Thumbnail Image.png
Description

The COVID-19 pandemic has resulted in preventative measures and has led to extensive changes in lifestyle for the vast majority of the American population. As the pandemic progresses, a growing amount of evidence shows that minority groups, such as the Deaf community, are often disproportionately and uniquely affected. Deaf

The COVID-19 pandemic has resulted in preventative measures and has led to extensive changes in lifestyle for the vast majority of the American population. As the pandemic progresses, a growing amount of evidence shows that minority groups, such as the Deaf community, are often disproportionately and uniquely affected. Deaf people are directly affected in their ability to personally socialize and continue with daily routines. More specifically, this can constitute their ability to meet new people, connect with friends/family, and to perform in their work or learning environment. It also may result in further mental health changes and an increased reliance on technology. The impact of COVID-19 on the Deaf community in clinical settings must also be considered. This includes changes in policies for in-person interpreters and a rise in telehealth. Often, these effects can be representative of the pre-existing low health literacy, frequency of miscommunication, poor treatment, and the inconvenience felt by Deaf people when trying to access healthcare. Ultimately, these effects on the Deaf community must be taken into account when attempting to create a full picture of the societal shift caused by COVID-19.

ContributorsAsuncion, David Leonard Esquiera (Co-author) / Dubey, Shreya (Co-author) / Patterson, Lindsey (Thesis director) / Lee, Lindsay (Committee member) / Harrington Bioengineering Program (Contributor) / Department of Physics (Contributor) / Barrett, The Honors College (Contributor)
Created2021-05
Description

In this project, we aim to fabricate PIN structure-like diodes for radiation detectors using Boron Nitride (BN). This fabrication is done by performing lithography and metal deposition processes on a Cubic Boron Nitride (cBN) of around 200 nm in thickness layer on top of a boron doped diamond substrate. The

In this project, we aim to fabricate PIN structure-like diodes for radiation detectors using Boron Nitride (BN). This fabrication is done by performing lithography and metal deposition processes on a Cubic Boron Nitride (cBN) of around 200 nm in thickness layer on top of a boron doped diamond substrate. The main goal is to create the most efficient and affordable alpha particle—and ideally neutron—detector in a radiation setting. Thus, making more accessible radiation detectors that can be more easily produced and disposed of, as well as minimizing the size of conventional detectors.

ContributorsGutierrez, Eric (Author) / Nemanich, Robert (Thesis director) / Zaniewski, Anna (Committee member) / Barrett, The Honors College (Contributor) / Department of Physics (Contributor)
Created2023-05
131279-Thumbnail Image.png
Description
In this project we are analyzing the diamond-titanium interface as it applies to diamond-based diode devices, including alpha particle, proton, and neutron detectors. This is done through the fabrication of an O-terminated B-doped diamond sample with a 20 Å Ti / 10 Å Pt overlayer which was then annealed and

In this project we are analyzing the diamond-titanium interface as it applies to diamond-based diode devices, including alpha particle, proton, and neutron detectors. This is done through the fabrication of an O-terminated B-doped diamond sample with a 20 Å Ti / 10 Å Pt overlayer which was then annealed and examined via X-ray photoelectron spectroscopy (XPS). It was discovered that after annealing the sample at temperatures ranging from 400 C - 900 C that TiC was not formed at any point during this experiment. Possible reasons for this include a lack of sufficient titanium in order to form TiC and over oxygenating the diamond surface before the metal was deposited.
ContributorsJohnson, Holly (Author) / Zaniewski, Anna (Thesis director) / Nemanich, Robert (Committee member) / Department of Physics (Contributor) / Barrett, The Honors College (Contributor)
Created2020-05